Description for 3M 413DL
Double coated tape designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive systems are specially formulated<br/>for clean removability from both the plate and the print cylinder.Chemical Resistance Chemical Resistance: Fluid Resistance: Excellent Water resistance, Good Alkanes, Chemical Resistance: Fair Alcohols Application Type Bond 1 Part or 2 Part 1-Part Material Form Double Coated Tape Substrate Composite Sleeve, Stainless Steel, Rubber Industry Printing solids and line work, Flexographic Printing Cylinders Manufacturer 3M Chemistry Rubber Firm Cure Method Pressure Sensitive Color Black High Temperature Resistance (°C) 54 Density (g/cm³) 1.060 -
Technical Data for 3M 413DL
Overview
-
Chemical Resistance
- Chemical Resistance : Fluid Resistance : Water Resistance - Excellent Water resistance
- Chemical Resistance - Good Alkanes
- Chemical Resistance : Relative Solvent Resistance - Fair Alcohols
-
Application Type
- Adhesive - Bond
-
1 Part or 2 Part
- 1-Part
-
Material Form
- Tape - Double Coated Tape
-
Substrate
- Rubber
- Composites - Composite Sleeve
- Stainless Steel
- Other - Photopolymer
-
Industry
- Printing and Graphics - Flexographic Printing Cylinders, Printing solids and line work
-
Chemistry
- Other - Rubber Firm
-
Cure Method
- Pressure Sensitive (min) - Pressure Sensitive
-
Color
- Black
Specifications
Bond Strength
Peel Strength (piw) 40 (oz/in), 25 (oz/in), 30 (oz/in), 50 (oz/in) Test Method Shear Strength (psi) 1000 (grams), 250 (grams) Test Method Material Resistance
High Temperature Resistance (°C) 54 Other Properties
Density (g/cm³) 1.060 Business Information
Shelf Life (mon) 12 -
-
Best Practices for 3M 413DL
-
Comparable Materials for 3M 413DL
Spec Engine® Results
Popular Articles
Infographic: ENSURING A STRONG BOND - 6 Basic Methods of Surface Preparation
Read ArticleLightweighting drives automotive adhesives demand
Read ArticleTesting the effectiveness of surface treatments
Read Article6 objects held together by adhesives you probably can't live without
Read ArticleSponsored Articles
Unique Advantages of Contact Adhesives
Read ArticleUsing LOCTITE® 454™ is a Valid Option for Engineers Working with a Wide Variety of Materials
Read ArticleSylgard 184 by DOW is the Top Choice for a Transparent, Silicone Encapsulant. Read Why:
Read ArticleCase Study: Creating reliable, corrosion-free bonds with LORD® 406 acrylic adhesive
Read ArticleFeatured Ads

Shear Strength Test Methods
Shear Strength | Type | Test Time | Test Temperature | Test Method |
---|---|---|---|---|
1000 (grams) | Static shear strength | 600,000 sec | 20°C Room Temperature | Value is weight that tape will hold for 10,000 minutes (ASTM D-3654) |
250 (grams) | Static shear strength | 600,000 sec | 70°C | Value is weight that tape will hold for 10,000 minutes (ASTM D-3654) |
Peel Strength Test Methods
Peel Strength | Substrate | Test Method |
---|---|---|
40 (oz/in) | Stainless Steel | ASTM D-3330 |
25 (oz/in) | Composite Sleeve | ASTM D-3330 |
30 (oz/in) | Photopolymer | ASTM D-3330 |
50 (oz/in) | Rubber | ASTM D-3330 |