Description for Elantas (Altana) Easypoxy K-22
A black, two-component, 100%-solids, room temperature cure epoxy adhesive system. General-purpose adhesive and repair compound for metal, wood, rubber and most plastics.<br/>Brand Cytec, Easypoxy Application Type Bond, Repair, Seal 1 Part or 2 Part 2 Part Material Form Paste Substrate Etched aluminum, Metal, Most plastics , Rubber, Wood, Aluminum Industry General purpose Manufacturer Elantas (Altana) Chemistry Solventless Application Method Spatula Cure Method Low heat cure, Room temperature cure Cure Temperature (°C) 20 to 25 Room temperature, 25, 65 Cure Time (min) 1,440, 120 Color Black, Clear Fungus Resistance Fungus Resistance
Popular Articles
Testing the effectiveness of surface treatments
Read ArticleInfographic: ENSURING A STRONG BOND - 6 Basic Methods of Surface Preparation
Read ArticleWhat Are the Differences Between Adhesives and Sealants?
Read ArticleAnaerobic Adhesives
Read ArticleSponsored Articles
Unique Advantages of Contact Adhesives
Read ArticleUsing LOCTITE® 454™ is a Valid Option for Engineers Working with a Wide Variety of Materials
Read ArticleSylgard 184 by DOW is the Top Choice for a Transparent, Silicone Encapsulant. Read Why:
Read ArticleCase Study: Creating reliable, corrosion-free bonds with LORD® 406 acrylic adhesive
Read ArticleFeatured Ads

Linear Shrinkage Test Methods
Linear Shrinkage | Test Method | Temp |
---|---|---|
<1.00 % | ASTM D2566 | 25°C |
Compressive Strength Test Methods
Compressive Strength | Test Temperature | Test Method |
---|---|---|
10,000 psi | 25°C | ASTM D695 |
Flexural Strength Test Methods
Flexural Strength | Test Temperature | Test Method |
---|---|---|
6,000 psi | 25°C | ASTM D790 |
Tensile Strength Test Methods
Tensile Strength | Substrate | Test Temperature | Test Method |
---|---|---|---|
2,500 psi | Etched AL/AL | 25°C | |
1,600 psi | Etched AL/AL | -55°C | |
2,300 psi | Etched AL/AL | 82°C | |
3,000 psi | 25°C | ASTM D412 |
Shear Strength Test Methods
Shear Strength | Type | Substrate | Test Temperature | Test Method |
---|---|---|---|---|
2,500 psi | Lap Shear strength | Etched aluminum /aluminum | 25°C | ASTM D1002 |
1,600 psi | Lap Shear strength | Etched aluminum /aluminum | -55°C | ASTM D1002 |
2,300 psi | Lap Shear strength | Etched aluminum /aluminum | 82°C | ASTM D1002 |
Dielectric Constant Test Methods
Dielectric Constant | Temperature | Test Method |
---|---|---|
4.60 | 25°C | 1 kHz, ASTM D150 |
Dissipation Factor Test Methods
Dissipation Factor | Temperature | Test Method |
---|---|---|
0.01000 | 25°C | 1 kHz, ASTM D150 |
Thermal Conductivity Test Methods
Thermal Conductivity | Test Method |
---|---|
5.7 (cal/sec/cm2/°C/cm x 10-4) |
Volume Resistivity Test Methods
Volume Resistivity | Temp (°C) | Test Method |
---|---|---|
4.0e13 (ohm-cm) | 25°C | ASTM D257 |
Shore D Hardness Test Methods
Shore D Hardness | Shore Hardness Test Method | Hardness Temperature |
---|---|---|
85 | ASTM D2240 | 25°C |